【Предыдущее】 | 【Следующее】 |
![]() |
![]() |
![]() |
![]() ![]() ![]() ![]() ![]() |
KAPTON COPPER MAGNET WIRE
Production Process
|
|
|
Step 1:Extruding&Drawing Incoming quality control for each material under strict standards.
|
|
|
|
|
|
Step 4:Wind Using two-way stretched F46 polyimide film to lapping the conductor. Min breakdown voltage can reach 12000v.
|
|
|
|
![]() |
Packing:Plastic spool, Wooden spool and according to customers requirements.
Test of Main technical
Standard |
JB5331-91 |
||
Test Item |
Requirement |
Test Result |
|
Appearance |
Uniform color smooth surface |
Uniform color smooth surface |
|
Insulation Thickness |
≤0.3mm |
|
|
Elongation |
≥25% |
40% |
|
Bending |
4A 4B |
No film-cracking |
|
Adhesion |
Stretching 15% (≤1b) |
Qualified |
|
Heat shock |
220C / 240C 30min 3a |
No film-cracking |
|
Breakdown voltage |
≥12000V |
|